Taking silica aerogels and polytetrafluoroethylene as additives and glass fiber as reinforcement,the effects of different glass fiber content on the properties of silica aerogels/PTFE composite insulation panels were investigated.The structure and properties of the composites were characterized by FT-IR,BET and comprehensive thermal analysis.The results shown that when the glass fiber content was 1.5wt%,the overall performance of the composites was the best,and the pore diameter was 116.90nm.In addition,the density of the composites increased linearly with the increase of the amount of glass fiber.With the increase of the amount of glass fiber,the high temperature resistance of the composites became stronger and the thermal conductivity changed less and less.
Li De, Huang Dongmei, Chen Chen, Shen Yiming, Wang Chaoyi, Yuan Qi, Hu Yiwei, Shao Danni
. Influence of glass fiber on structure and property of reinforced aerogel composite[J]. New Chemical Materials, 2021
, 49(7)
: 122
-125
.
DOI: 10.19817/j.cnki.issn 1006-3536.2021.07.028
[1] 郑文芝.二氧化硅气凝胶研制及其结构性能研究[D].广州:华南理工大学,2010.
[2] 陈姚,酆赵龙,黄湘桦.纳米二氧化硅气凝胶隔热材料的研究进展[J].无机盐工业,2010,42(11):4-6.
[3] 李明明,王坤杰,张晓虎.纤维增强SiO2气凝胶复合材料研究进展[J].化工新型材料,2017,45(3):19-21.
[4] 秦国彤,门薇薇,魏微.气凝胶研究进展[J].材料科学与工程学报,2005(2):293-296.
[5] 余煜玺,吴晓云,伞海生.常压干燥制备疏水性SiO2-玻璃纤维复合气凝胶及表征[J].材料工程,2015,43(8):31-36.
[6] 谢苏江.聚四氟乙烯的改性及应用[J].化工新型材料,2002,30(11):26-30.
[7] 张文举,朱宇雄,张文艺.玻璃微珠对改性聚四氟乙烯密封板材性能影响的研究[J].中国塑料,2005(6):63-66.
[8] Khedkar,Jaydeep,Negulescu.Sliding wear behavior of PTFE composites[J].Wear,2002,252(5):361-369.
[9] Sawyer W G,Freudenberg K D,Bhimaraj P,et al.A study on the friction and wear behavior of PTFE filled with Alumina Nanoparticles[J].Wear,2003,254(5):573-580.
[10] 黄丽,杨儒,郭江江.微米和纳米SiO2改性聚四氟乙烯的摩擦磨损性能[J].复合材料学报,2004,21(4):82-86.
[11] 王家序,陈战,秦大同.聚四氟乙烯复合材料的摩擦磨损性能研究[J].农业机械学报,2002,33(4):99-101.
[12] 贾均红,陈建敏,周惠娣.炭纤维增强聚四氟乙烯复合材料在干摩擦和水润滑条件下的摩擦学行为对比研究[J].摩擦学学报,2004,24(1):16-20.
[13] 李如琰.聚四氟乙烯纤维织物在关节轴承上的应用[C].中国功能材料及其应用学术会议,2004.
[14] 王兵,王应德.超细碳纤维增强二氧化硅气凝胶的隔热性能研究[C].中国空间科学学会空间材料专业委员会学术交流会议论文,2012.
[15] Abe I,Sato K,Abe H,et al.Formation of porous fumed silica coating on the surface of glass fibers by a dry mechanical processing technique[J].Advanced Powder Technology,2008,19(4):311-320.
[16] Ristic-Lehmann C,Farnworth B,Dutta A,et al.Materiau isolant composite aerogel/ptfe:WO,WO2005047381 A1[P].2005-05-26.
[17] Watanabe M.Wear mechanism of PTFE composites in aqueous environments[J].Wear,1992,158(1-2):79-86.
[18] Klaas N V,Marcus K,Kellock C.The tribological behaviour of glass filled polytetrafluoroethylene[J].Tribology International,2005,38(9):824-833.
[19] Lancaster J.Accelerated wear testing of PTFE composite bearing materials[J].TribologyInternational,1979,12(2):65-75.
[20] Randall J P,Meador M A,Jana S C.Tailoring mechanical properties of aerogels for aerospace applications[J].ACS Appl Mater Interfaces,2011,3(3):613-626.