Research status and development trend of aircraft thermal protection material

Expand
  • 1.School of Textile Science and Engineering,Tianjin Polytechnic University,Tianjin 300387;
    2.Key Laboratory of Advanced Textile Composites of Ministry of Education,Tianjin Polytechnic University,Tianjin 300387

Online published: 2020-12-07

Abstract

Thermal protection is one of the most important technologies in the aerospace field.In the face of harsh exploration environment and ultra-high speed flight,thermal protection materials need to be developed urgently.The basic characteristics and development of carbon/carbon composites,ultra-high temperature ceramics and their composites were reviewed.The advantages and disadvantages of the existing aircraft thermal protection materials were compared and analyzed,and looking forward to its future development direction.

Cite this article

Wang Jiawei, Zheng Zhenrong, Bi Yuejiao . Research status and development trend of aircraft thermal protection material[J]. New Chemical Materials, 2020 , 48(11) : 15 -19 . DOI: 10.19817/j.cnki.issn 1006-3536.2020.11.004

References

[1] 邹军锋,李文静,刘斌,等.飞行器用热防护材料发展趋势[J].宇航材料工艺,2015,45(4):10-15.
[2] 张志刚.高超声速飞行器热防护系统设计方法[D].哈尔滨工业大学硕士学位论文,2014.
[3] 鲁芹,姜贵庆,罗晓光,等.X-37B空天飞行器轻质非烧蚀热防护新技术[J].现代防御技术,2012,40(1):16-20.
[4] Blosser M,Chenr,Schmidt I,et al.Advanced metallicthermal protection systems development[J].AIAA-2002-0504.
[5] 邢亚娟,孙波,高坤,等.航天飞行器热防护系统及防热材料研究现状[J].宇航材料工艺,2018,48(4):9-15.
[6] 张力川.碳碳复合材料发展现状及前景探索[J].建材与装饰,2016(8):125-126.
[7] Park S J,Seo M K,The effects of MoSi2 on the oxidation behavior of carbon/carbon composites[J].Carbon,2001,39(8):1229-1235.
[8] 曾燮榕,李贺军,李龙,等.碳/碳复合材料MoSi2/SiC涂层在动态氧化环境下的性能研究[J].复合材料学报,2002,19(6):43-46.
[9] Huang J F,Zeng X R,Li H J,et al.ZrO2-SiO2 gradient multi-layeroxidation protective coating for SiC coated carbon/carbon composites[J].Surface & Coating Technology,2005,190(2/3):255-259.
[10] 王铭辉.碳纤维复合材料在航空航天领域的应用研究[J].现代商贸工业,2019,40(8):191-193.
[11] 陶肖明.纺织结构复合材料[M].北京:科学出版社,2001.
[12] 苏君明,周绍建,李瑞珍,等.工程应用C/C复合材料的性能分析与展望[J].新型炭材料,2015,30(2):106-114.
[13] 孙乐,王成,李晓飞,等.C/C复合材料预制体的研究进展[J].航空材料学报,2018,38(2):86-95.
[14] Chen Y,Wang C G,Zhao W.Influence of SiC whisker on formation and oxidation resistance of coating for C/C composite[J].Advanced Materials Research,2012,430:373-377.
[15] Jiao G S,Li H J,Li K Z,et al.Study on the oxidation mechanism of the coated C/C composites[J].Journal of Functional Materials,2007,38(8):1327-1330.
[16] Jiao X,Li T,Li Y,et al.Oxidation behavior of SiC/glaze-precursor coating on carbon/carbon composites[J].Ceramics International,2017.
[17] Jin X,Fan X,Lu C,et al.Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites[J].Journal of the European Ceramic Society,2017,42:1356-1363.
[18] Kuo H H,Lin J H C,Ju C P.Effect of carbonization rate on the properties of a PAN/phenolic-based carbon/carbon composite[J].Carbon,2005,43(2):229-239.
[19] La Forest M L,Parker C A,Dillon F,et al.Manufacture of functionally graded carbon-carbon composites:US,US7063870[P].2006.
[20] Worrell L W.High temperature alloys:US6127047[P].2000-10-3.
[21] 承涵.C/C复合材料表面双辉W/Ir复合涂层及其组织结构研究[D].南京:南京航空航天大学,2010.
[22] Fang H T,Zhu J C,Yin Z D,et al.A Si-Mo fused slurry coating for oxidation protection of carbon-carbon composites[J].Journal of Materials Science Letters,2001,20(2):175-177.
[23] Zhang H,Zhu L A,Bai S X,et al.Ablation-resistant Ir/Re coating on C/C composites at ultra-high temperatures[J].Rare Metals,2015:1-10.
[24] 黄剑锋,李贺军,熊信柏,等.炭/炭复合材料高温抗氧化涂层的研究进展[J].新型炭材料,2005,20(4):373-379.
[25] 曾毅,张武装,熊翔.C/C复合材料SiC/ZrB-2-MoSi-2复合涂层的抗氧化机制[J].复合材料学报,2010,27(3):50-55.
[26] 张伟刚,成会明,沈祖洪,等.碳化硅抗氧化涂层的失效分析[J].新型碳材料,1998(2):12-16.
[27] 王俊山,李仲平,敖明,等.掺杂难熔金属碳化物对炭/炭复合材料烧蚀微观结构的影响[J].新型炭材料,2005(2):97-102.
[28] 郭麒.C/C复合材料表面CoNiCrAlTaHfY/Co涂层及其高温氧化性能研究[D].太原理工大学,2018.
[29] 付前刚,李贺军,黄剑锋,等.炭/炭复合材料磷酸盐涂层的抗氧化性能研究[J].材料保护,2005(3):52-54,75.
[30] Huang J F,Zhang Y L,Zhu K J,et al.Microstructure and oxidation protection of borosilicate glass coating prepared by pulse arc discharge deposition for C/C composites[J].Ceramics International,2014,41(3):4662-4667.
[31] Fu Q G,Zhuang L,Ren Q W,et al.Carbon nanotube-toughened interlocking buffer layerto improve the adhesion strength and thermal shock resistance of SiC coating forC/C-ZrC-SiC composites[J].Journal of Materiomics,2015,1(3).
[32] Messinger R,Pulley J.Thermal-mechanical cycle test of a cryogenic tank of RLV[R].AIAA-2003-1766.
[33] 张磊磊,付前刚,李贺军.超高温材料的研究现状与展望[J].中国材料进展,2015,34(9):675-683.
[34] Levines R,Opila E J,Halbig M C,et al.Evaluation of ultra-high temperature ceramics for aeropropulsionuse[J].Journal of the European Ceramic Society,2002,22(14/15):2757-2767.
[35] 齐方方,王子钦,李庆刚,等.超高温陶瓷基复合材料制备与性能的研究进展[J].济南大学学报(自然科学版),2019,33(1):8-14.
[36] 杨文慧.Zr、Hf系超高温陶瓷抗氧化烧蚀性能研究[D].北京:北京理工大学,2016.
[37] Ma B X,Han W B.Thermal shock resistance of ZrC matrix ceramics[J].Journal of Refractory Metals and Hard Materials,2010,28:187-190.
[38] 刘晗.碳化硅添加剂对碳化钽陶瓷显微组织及力学性能的影响[D].哈尔滨:哈尔滨工业大学,2013.
[39] Kljajevic L,Nenadovic S,Nenadovic M,et al.Spark plasma sintering of ZrC-SiC ceramics with LiYO2additive[J].Ceramics International,2013,39:5467-5476.
[40] Feng L,Lee S H,Kim H N.Effects of high-energy ball milling and reactive spark plasma sintering on the densification of HfC-SiC composites[J].Journal of the European Ceramic Society,2017,37(5):1891-1898.
[41] 郭强强,冯志海,周延春.超高温陶瓷的研究进展[J].宇航材料工艺,2015(5):1-13.
[42] Ni D W,Liu J X,Zhang G J.Microstructure refinement and mechanical properties improvement of HfB2-SiC composites with the incorporation ofHfC[J].Journal of the European Ceramic Society,2012,32(10):2557-2563.
[43] Jin H,Meng S H,Zhang X H,et al.Effectsof oxygen partial pressure on the oxidation of ZrB2-SiC-graphite composites at 1800℃[J].Ceramics International,2016,42(5):6480-6486.
[44] Zhang J P,Fu Q G,Wang L.Preparation,ablation behavior and thermal retardant ability of C-C-HfB2-SiC composites[J].Materials & Design,2017,132:552-558.
[45] 王一博,刘振国,胡龙,等.三维编织复合材料研究现状及在航空航天中应用[J].航空制造技术,2017(19):78-85.
[46] 张幸红,胡平,韩杰才,等.超高温陶瓷复合材料的研究进展[J].科学通报,2015,60(3):257-266.
Options
Outlines

/