Study on repair technology of skin-core flaw in functional composite sandwich structure

Expand
  • 1. State-owned Wuhu Machinery Factory,Wuhu 241000;
    2. Key Laboratory of Plasma Dynamics,Air Force Engineering University,Xi'an 710038

Received date: 2020-08-26

  Revised date: 2021-09-10

  Online published: 2021-12-31

Abstract

The intact and skin-core flaw with a diameter of 30mm samples of functional composite electromagnetic absorbing honeycomb sandwich were designed and prepared removed the skin of the samples' skin-core debonding area at a slope of 1∶15 by a pneumatic grinding tool.The J-116A adhesive film and QW280/5429 prepreg patch were laid for bonding repair after the flaws were removed,the repair area of the samples were heated and solidified by using a hot bonder.Ultrasonic nondestructive testing,electromagnetic reflectivity in the frequency range of 1~18GHz,flat tensile strength test and bending strength test of the samples were carried out.The results showed that,the recovery rate of repaired samples' effective electromagnetic absorption bandwidth reached to 96.8%,the recovery rate of flat tensile strength reached to 85.5%,the recovery rate of bending strength reached to 95.1%,the adhesive film,prepreg patch and skin-core bonding in repair area on the samples were of good quality.

Cite this article

Ji Guoliang, Li Yiwen, Xuan Shanyong, Wei Xiaolong, Chen Ge . Study on repair technology of skin-core flaw in functional composite sandwich structure[J]. New Chemical Materials, 2021 , 49(12) : 227 -231 . DOI: 10.19817/j.cnki.issn 1006-3536.2021.12.048

References

[1] 宫元勋,欧秋仁,赵宏杰,等.吸波蜂窝复合材料的结构优化和吸波性能研究[C].北京:第17届全国复合材料学术会议论文,2012.
[2] 杜善义.先进复合材料与航空航天[J].复合材料学报,2007,24(1):1-12.
[3] 礼嵩明,吴思保,王甲富,等.含超材料的新型蜂窝夹层结构吸波复合材料[J].航空材料学报,2019,39(3):94-99.
[4] 赵宏杰,嵆培军,胡本慧,等.蜂窝夹层复合材料的吸波性能[J].宇航材料工艺,2010,40(2):72-76.
[5] 陈绍杰.复合材料结构修理指南[M].北京:航空工业出版社,2001.
[6] 常霞,袁昊,高正平.蜂窝夹芯吸波材料电磁特性研究进展[J].磁性材料及器件,2013,44(5):73-76.
[7] Duong C N,Wang C H.Composite repair theory and design[M].The Netherlands:Elsevier BV,2007.
[8] 李江海,孙秦.结构型吸波材料及其结构型式设计研究进展[J].机械科学与技术,2003,22(z1):188-190.
[9] 刘丛丛.高性能复合材料发展展望[J].化工新型材料,2012,40(1):1-3.
[10] Armstrong K B.Care and repair of advanced composites[M].Second edition.US:SAE International,2005,l43-147.
[11] 包啸,龚志红,何凯,等.复合材料泡沫夹层结构板-芯缺陷挖补修补工艺研究[J].化工新型材料,2020,48(5):164-167.
[12] 郭霞,关志东,刘遂,等.蜂窝夹层修理结构的弯曲性能试验分析[J].复合材料学报,2013,30(5):187-194.
[13] Tomblin J S,Salah L,Welch J M.Bonded repair of aircraft composite sandwich structures,DOT/FAA/AR~03/74[R].Washington DC:Office of Aviation Research,2004.
[14] 汪海,陈秀华,郭杏林,等.复合材料蜂窝夹芯结构修理后强度研究[J].航空学报,2001,22(3):270-273.
[15] 周银华,赵美英,王瑜,等.含穿透损伤复合材料蜂窝夹芯修补结构强度分析[J].西北工业大学学报,2011,29(4):536-541.
[16] Belouettar S,Abbadi A,Azari Z,et al.Experimental investigation of static and fatigue behaviour of composites honeycomb materials using four point bending tests[J].Composite Structures,2009,87(3):265-273.
[17] He Li,Cheng Yuansheng,Liu Jun.Precise bending stress analysis of corrugated-core honeycomb-core and X core sandwich panels[J].Composite Structures,2012,94(5):1656-1668.
Options
Outlines

/