核空气净化用浸渍活性炭的中毒老化效应及影响因素分析
王坤俊1, 王龙江1, 韩丽红1, 樊惠玲2, 俞杰1
1.中国辐射防护研究院环境工程技术研究所,太原030006;
2.太原理工大学煤科学与技术教育部和山西省重点实验室,太原030024
Influence factor on poisoning and aging of impregnated activated carbon for nuclear air cleaning
Wang Kunjun1, Wang Longjiang1, Han Lihong1, Fan Huiling2, Yu Jie1
1.Department of Environmental Engineering Technology,China Institute for Radiation Protection,Taiyuan 030006;
2.Key Laboratory of Coal Science and Technology,Ministry of Education and Shanxi Province,Taiyuan University of Technology,Taiyuan 030024
下载:  PDF (1292KB) 
输出:  BibTeX | EndNote (RIS)      
摘要 碘吸附器是核电站等核设施空气净化系统的关键设备,主要由金属壳体和内部装填的浸渍活性炭组成。浸渍活性炭受多种因素影响而引起的中毒老化效应,是导致碘吸附器及浸渍活性炭净化效率下降的主要原因。对中毒和老化条件下浸渍活性炭吸附放射性甲基碘效率进行了研究,利用N2吸附进行了老化活性炭的孔结构分析,并进一步分析了造成浸渍活性炭中毒和老化的影响原因。研究发现,使用3年以上的浸渍活性炭的吸附效率开始下降,老化时间越长,效率越低;老化对浸渍活性炭孔结构造成不利影响,但对浸渍剂的影响是浸渍活性炭效率下降的主要原因。
服务
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章
王坤俊
王龙江
韩丽红
樊惠玲
俞杰
关键词:  核空气  净化  浸渍活性炭  中毒老化  吸附性能    
Abstract: Iodine absorber is a key component of ventilation and off-gas treatment system of nuclear power plant and other nuclear facility,it consists mainly of metal shell and internal impregnated activated carbon.The impregnated activated carbon is caused poisoning and aging effects by a variety of factors,which is the main factor leading to the purification efficiency decline of iodine adsorber and impregnated activated carbon.The adsorption efficiency of radioactive methyl iodide of impregnated activated carbon in different aging conditions were studied,the pore structure of aged activated carbon was analyzed by N2 adsorption,and the main influencing factors of activated carbon poisoning and aging were analyzed.The study found that the efficiency of carbon for more than three years began to decline,the longer the aging time was,the lower the efficiency was.With the use of environment and time,the decline of efficiency was also different.The aging of activated carbon produced a certain adverse effect on itself pore structure,and the influence of poisoning and aging on the impregnation should be the main reason for the decrease in the efficiency.
Key words:  nuclear air    cleaning    impregnated activated carbon    poisoning and aging    adsorption property
收稿日期:  2017-07-13                     发布日期:  2018-11-05      期的出版日期:  2018-09-20
基金资助: 国家自然科学基金项目(21576180);山西省应用基础研究计划项目(201701D221095)
作者简介:  王坤俊(1984-),男,硕士,助理研究员,研究方向为核空气净化理论与技术。
引用本文:    
王坤俊, 王龙江, 韩丽红, 樊惠玲, 俞杰. 核空气净化用浸渍活性炭的中毒老化效应及影响因素分析[J]. 化工新型材料, 2018, 46(9): 190-194.
Wang Kunjun, Wang Longjiang, Han Lihong, Fan Huiling, Yu Jie. Influence factor on poisoning and aging of impregnated activated carbon for nuclear air cleaning. New Chemical Materials, 2018, 46(9): 190-194.
链接本文:  
http://www.hgxx.org/CN/  或          http://www.hgxx.org/CN/Y2018/V46/I9/190
[1]核工业标准化研究所.NB/T 20039.11—2011核空气和气体处理规范 通风、空调与空气净化第11部分:碘吸附器(Ⅰ型)[S].北京:原子能出版社,2011:2-8.
[2]Wilhelm J.Development and application of filters for air cleaning in nuclear power plants[J].Nuclear Engineering and Design,1987,103(1):139-147.
[3]Sachin U N,Kai C,Vivek U,et al.Capture of harmful radioactive contaminants from off-gas stream using porous solid sorbents for clean environment-a review[J].Chemical Engineering Journal,2016,306:369-381.
[4]Zhou J,Hao S,Gao L,et al.Study on adsorption performance of coal based activated carbon to radioactive iodine and stable iodine[J].Annals of Nuclear Energy,2014,72:237-241.
[5]Hou X,Andersson K G,Roed J,et al.Dry deposition of elemental iodine on skin,hair,and clothing from air[J].Journal of Radioanalytical and Nuclear Chemistry,2007,271(1):133-143.
[6]Kevin W W.Phase I aging assessment of nuclear air-treatment system high efficiency particulate air and adsorbers[J].Nuclear Engineering and Design,1996(163):315-322.
[7]Broadbent D.The ageing and poisoning of charcoal used in nuclear plant air cleaning systems[C].CEC European Conference on Gaseous Effluent Treatment in Nuclear Installations,Luxembourg:Graham and Trotman,1985:14-18.
[8]Billinge B H M.The desorption of chemisorbed oxygen from activated carbons and its relationship to ageing and methyl iodide retention efficiency[J].Carbon,1984(22):84-89.
[9]Deuber H,Gerlach K.Investigations on the aging of activated carbons in the exhaust air of a pressurized water[J].Reactor Nucl Techn,1985(70):161-169.
[10]Wilhelm J.Development and application of filters for air cleaning in nuclear power plants[J].Nuclear Engineering and Design,1987,103(1):139-147.
[11]American society for testing and materials.ASTM D3803-98 standard test method for nuclear-grade activated carbon[S].Philadelphia,PA:ASTM International,1998.
[12]核工业标准化研究所.EJ/T 20056—2014核级活性炭去除甲基碘性能试验方法[S].北京:原子能出版社,2014:2-10.
[13]Rastunov L N,Magomedbekov E P,Obruchikov A V.Evaluation of the sorbent layer thickness in iodine filters[J].Atomic Energy,2011,110(1):68-72.
[14]Wilhelm J G.Iodine filters in nuclear installations.Luxemburg[C].Commission of the European Communities,1982:125-126.
[15]González-García C M,Roman S.Surface free energy analysis of adsorbents used for radioiodine adsorption[J].Applied Surface Science,2013(282):714-717.
[16]Gregory W,Peterson J A.Effects of water on the removal of methyl bromide using triethylenediamine impregnated carbon[J].Carbon,2010(48):81-88.
[17]Nacapricha D,Taylor C G.Quality control of nuclear charcoals:particle size effect and trapping mechanism[J].Carbon,1996(34):l55-163.
[18]González-García C M,González J F.Removal efficiency of radioactive methyl iodide on TEDA-impregnated activated carbons[J].Fuel Processing Technology,2011(92):247-252.
[19]Park S W,Lee W K.Adsorption and desorption of gaseous methyl iodide in a triethylenediamine-impregnated activated carbon bed.Separations[J].Technology,1993,3(3):133-142.
[1] 丁赛赛, 刘高旗, 许红亮, 杨碧野. KOH活化法制备煤基活性炭及其吸附性能研究[J]. 化工新型材料, 2018, 46(4): 157-160.
[2] 曾月, 敬雪莲, 李慧霖, 付珍珍, 李俣珠, 陈姝娟, 何利, 刘书亮, 周康. 羧甲基半纤维素/壳聚糖复合材料的制备及其对Cu2+的吸附性能研究[J]. 化工新型材料, 2018, 46(4): 165-168.
[3] 李婷, 李欣桐, 李敏, 吴琪琳. 山竹壳基生物质活性炭的制备及其吸附性能研究[J]. 化工新型材料, 2018, 46(2): 213-216.
No Suggested Reading articles found!
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
京ICP备09035943号-38
版权所有 © 《化工新型材料》编辑部
本系统由北京玛格泰克科技发展有限公司设计开发 技术支持:support@magtech.com.cn